Start with the first layer
Most failed prints fail in the first layer. Before anything else, check the bed is clean (wash PEI with dish soap or wipe with isopropyl alcohol), the nozzle height is right (lines slightly squashed, not round or transparent), and the first layer is printed slowly.
Problems, causes and fixes
| Problem | What you see | Likely causes | Try first |
|---|---|---|---|
| Poor bed adhesion | Print detaches or drags | Dirty bed, nozzle too high, bed too cold | Clean the bed, re-level / Z-offset, raise bed temperature, add a brim |
| Warping | Corners lift and curl | Material shrinkage, drafts, cold bed | Enclosure (ABS/ASA), brim, chamfer bottom edges, correct bed temperature |
| Stringing | Hair-like threads between parts | Oozing during travel, wet filament, too hot | Tune retraction, lower temperature 5–10 °C, dry the filament |
| Under-extrusion | Gaps, thin walls, weak parts | Partial clog, wet filament, speed above hotend flow, wrong E-steps | Lower speed, check flow, clean nozzle, calibrate E-steps |
| Over-extrusion | Blobby, oversized parts | Flow too high, wrong filament diameter setting | Calibrate flow; check 1.75 vs 2.85 mm setting |
| Layer shifts | Layers suddenly offset | Loose belt or pulley, collisions, too fast | Tighten belts and pulley screws, reduce acceleration |
| Elephant’s foot | First layers bulge outward | Nozzle too close, bed too hot | Raise Z slightly, lower bed temperature, add a bottom chamfer |
| Ghosting / ringing | Echo ripples after corners | Vibration at high acceleration | Lower acceleration/jerk; input shaping if your firmware supports it |
| Zits and blobs | Spots on walls | Seam placement, pressure changes | Align or randomise the seam, tune retraction / pressure advance |
| Drooping overhangs and bridges | Saggy undersides | Not enough cooling, too hot, too steep | More fan, slower bridges, supports, reorient |
Calibrate once, save time forever
A handful of short tests remove most guesswork:
- E-steps — the extruder must push what it is told. Use the E-steps calculator.
- Flow / extrusion multiplier — print a single-wall box and measure the wall.
- Temperature — print a temperature tower and choose the cleanest band.
- Retraction — tune distance and speed to stop stringing.
- Overhangs and bridges — print our overhang test and bridging test.
- Dimensions and fit — print a tolerance gauge and use the shrinkage calculator for any scaling error.
When the file is the problem
Some failures come from the model, not the machine: missing walls, gaps in the toolpath, or slices that look empty. Open the file in the 3D Studio — open edges, non-manifold edges and inside-out shells are listed and drawn. See Mesh repair.
Keep a log
Note the material, temperatures, speeds and what changed. One change at a time is the fastest way to a reliable profile.
Check your understanding
1. Hair-like threads between parts are called…
Usually fixed with retraction, temperature or drier filament.
2. Layers suddenly offset sideways usually point to…
Mechanical slip shifts the whole layer.
3. What should you check first for most failed prints?
Most failures start on layer one.