Quick chooser
| Material | Best for | Difficulty | Heat resistance |
|---|---|---|---|
| PLA | Prototypes, decor, most first prints | Easiest | Low — softens around 55–60 °C |
| PETG | Functional parts, outdoor-ish use, containers | Easy–moderate | Medium (~80 °C) |
| ABS | Tough parts, car interiors, acetone smoothing | Moderate–hard; needs enclosure | High (~100 °C) |
| ASA | Outdoor parts (UV resistant) | Moderate–hard; needs enclosure | High (~100 °C) |
| TPU | Flexible parts: gaskets, phone cases, tyres | Moderate; print slowly | Medium |
| Nylon (PA) | Gears, hinges, wear parts | Hard; must be kept dry | High |
| PC | Strong, heat-resistant parts | Hard; high temperatures | Very high (~140 °C) |
Typical print settings
| Material | Nozzle (°C) | Bed (°C) | Density (g/cm³) | Notes |
|---|---|---|---|---|
| PLA | 190–220 | 0–60 | 1.24 | Fan on; prints on most surfaces |
| PETG | 220–250 | 70–85 | 1.27 | Strings easily; slow travel and tune retraction |
| ABS | 230–260 | 90–110 | 1.04 | Enclosure; warps without it; ventilate |
| ASA | 240–260 | 90–110 | 1.07 | Like ABS with UV resistance |
| TPU (95A) | 210–230 | 30–60 | 1.21 | Slow speeds; direct-drive extruders help |
| Nylon | 240–270 | 70–90 | 1.14 | Dry before use; absorbs moisture fast |
| PC | 260–300 | 100–120 | 1.20 | All-metal hotend, enclosure |
These are typical ranges; always start from the spool manufacturer’s settings. Density lets you turn volume into weight — the filament calculator does it for you.
PLA: the default
PLA is stiff, easy, low-odour and available in every colour, including silk and matte finishes. Its weakness is heat: a PLA part in a hot car can deform. For cookie cutters, use a food-safe-rated filament and treat prints as single-season — layer lines can trap bacteria.
PETG: the practical upgrade
PETG is tougher and more heat- and chemical-resistant than PLA, with a little flex. It sticks extremely well — sometimes too well to smooth PEI or glass, where a release agent helps.
ABS and ASA: engineering classics
Strong and heat-resistant but they shrink as they cool, so large parts warp without an enclosure. Both emit fumes; print in a ventilated space.
TPU and flexibles
Rubber-like, measured by Shore hardness (95A is common and printable on most machines). Print slowly, minimise retraction and avoid long Bowden tubes.
Nylon, PC and composites
High-performance materials for gears and load-bearing parts. Carbon- or glass-fibre-filled versions are stiffer but abrasive: use a hardened nozzle.
Resins
Standard resins give fine detail but can be brittle; tough, flexible, castable and dental resins exist for specific jobs. See FDM vs resin vs SLS and the resin cost calculator.
Storage
Many filaments absorb moisture from the air, which causes popping, stringing and weak prints. Store spools sealed with desiccant; dry nylon, TPU and PETG before critical prints.
Check your understanding
1. Which filament is the easiest to start with?
PLA prints at low temperatures and rarely warps.
2. Which material is best for outdoor parts in sunlight?
ASA resists UV better than ABS.
3. Why should nylon be dried before printing?
Wet nylon pops and strings.